Add to Cart
0.58mm K type bare thermocouple wire alumel chromel wire for K type thermocouple cable or thermocouple sensor
TYPE K (CHROMEL vs ALUMEL ) is used in oxidizing, inert or dry reducing atmospheres. Exposure to vacuum limited to short time periods. Must be protected from sulfurous and marginally oxidizing atmospheres. Reliable and accurate at high temperatures.
1. Chemical Composition
Material | Chemical composition (%) | ||||
Ni | Cr | Si | Mn | Al | |
KP(Chromel) | 90 | 10 | |||
KN(Alumel) | 95 | 1-2 | 0.5-1.5 | 1-1.5 |
2. Physical properties and Mechnical properties
Material |
Density(g/cm3) |
Melting point℃) |
Tensile Strength(Mpa) |
Volume resistivity(μΩ.cm) |
Elongation rate (%) |
KP(Chromel) | 8.5 | 1427 | >490 | 70.6(20℃) | >10 |
KN(Alumel) | 8.6 | 1399 | >390 | 29.4(20℃) | >15 |
3. EMF Value range at different temperature
Material | EMF value Vs Pt(μV) | |||||
100℃ | 200℃ | 300℃ | 400℃ | 500℃ | 600℃ | |
KP(Chromel) | 2816~2896 | 5938~6018 | 9298~9378 | 12729~12821 | 16156~16266 | 19532~19676 |
KN(Alumel) | 1218~1262 | 2140~2180 | 2849~2893 | 3600~3644 | 4403~4463 | 5271~5331 |
EMF value Vs Pt(μV) | ||||
700℃ | 800℃ | 900℃ | 1000℃ | 1100℃ |
22845~22999 | 26064~26246 | 29223~29411 | 32313~32525 | 35336~35548 |
6167~6247 | 7080~7160 | 7959~8059 | 8807~8907 | 9617~9737 |
Hiedy Jiang
Ohmalloy Material Co., Ltd
Add: No. 1211, Mudanjiang Road, Baoshan district, Shanghai
TEL: +86-21-66796338 FAX: +86-21-66796339
Mob.: +86-186 4671 2628 Whatsapp/wechat: +86-186 4671 2628
Email: jiang@ohmalloy.com Web: www.ohmalloy.com